| Composition: | SiO₂ (Silicon Dioxide): ~80% |
| B₂O₃ (Boron Trioxide): ~12-13% | |
| Na₂O (Sodium Oxide) + K₂O (Potassium Oxide): ~4-5% | |
| Al₂O₃ (Aluminum Oxide): ~2-3% | |
| Thermal Properties | Softening Point: 820°C |
| Annealing Point: 560°C | |
| Strain Point: 520°C | |
| Maximum Operating Temperature: 500°C | |
| Thermal Expansion Coefficient (20°C to 300°C): 3.3 × 10⁻⁶ /°C | |
| Optical Properties | Refractive Index: 1.474 |
| Light Transmittance: >92% | |
| UV Cut-off Wavelength: ~290 nm | |
| Mechanical Properties | Density: 2.23 g/cm³ |
| Young's Modulus: 64 GPa | |
| Poisson's Ratio: 0.20 | |
| Bending Strength: 40 MPa | |
| Chemical Resistance: | Acid Resistance: Excellent Alkali Resistance: Good Hydrolytic Resistance: Class 1 (per ISO 719) |
| Alkali Resistance: Good | |
| Hydrolytic Resistance: Class 1 (per ISO 719) |